Blobs and zits are small bumps of extra plastic on the outside walls of a 3D print, and they almost always form where the nozzle stops, starts or changes direction: at the layer seam, after a travel move, or at a retraction. You fix them by hiding or spreading the seam, tuning retraction and wipe so the nozzle doesn’t ooze when it starts and stops, calibrating pressure advance, and making sure you aren’t over-extruding or printing with wet filament.
This guide explains what causes each kind of blob, how to tell them apart by where they sit on the part, and which settings to change in OrcaSlicer, Bambu Studio, PrusaSlicer and Cura. It applies to any FDM printer.
Quick fix checklist
Work down this list, re-printing the same small test part after each change:
- Look at where the zits are. Lined up in a vertical stripe means the seam. Scattered randomly means retraction, travel or wet filament.
- Move the seam to the back of the part, or to a sharp corner, with the seam position setting.
- Turn on wipe (PrusaSlicer, OrcaSlicer, Bambu Studio) or coasting (Cura) so the nozzle stops oozing before the end of the wall.
- Check retraction is in a sensible range: about 0.5–2 mm on direct drive, 4–7 mm on Bowden. Set any “extra length on restart” back to 0.
- Calibrate pressure advance (or linear advance) if your firmware supports it.
- Check flow. If walls are lumpy all over, you’re over-extruding.
- Dry the filament if you hear popping or crackling while it prints.
- Lower the nozzle temperature 5 °C at a time, staying in the filament’s range.
- Turn on avoid crossing walls so travel moves stay inside the part.
- Clean the nozzle so collected plastic can’t drop onto the print.
Ooze: a drop of molten plastic forming at the nozzle.Photo: David Elliott from UK ·CC BY 2.0 ·Wikimedia Commons
Molten plastic leaving the nozzle.Photo: David Elliott from UK ·CC BY 2.0 ·Wikimedia Commons
A thin strand pulled from the nozzle: where strings begin.Photo: David Elliott from UK ·CC BY 2.0 ·Wikimedia Commons
A brass 0.4 mm nozzle laying a thin strand.
A 20 mm calibration cube, often the first print.Photo: syvwlch ·CC BY 2.0 ·Wikimedia Commons
The calibration cube a few layers in.Photo: syvwlch ·CC BY 2.0 ·Wikimedia Commons
What are blobs and zits?
Zits (sometimes called pimples) are tiny bumps on the outer wall, often less than a millimetre across. Blobs are the same thing, larger. Both are small deposits of extra plastic left on the surface of the part.
Blobs, zits and faults that look similar
- Zits in a vertical line: the layer seam. Each layer starts and ends at the same spot, and the small bump there stacks up into a visible stripe.
- Zits scattered randomly: retraction, travel moves, wet filament, or the slicer placing the seam at random.
- Bulges at every corner: pressure building up as the nozzle slows into a corner. Pressure advance fixes this.
- Lumpy walls everywhere: general over-extrusion, not a stop-and-start problem.
- Thin strings between parts: stringing. It comes from the same oozing as zits, but shows up during travel instead of on the wall.
- A gap or dent at the seam: the opposite problem: too little plastic where the layer closes, often from too much wipe, coasting or retraction.
- The “blob of death”: a big lump of plastic that has leaked out and wrapped the hotend itself. That’s a leak or a print that came loose, not a surface defect. We cover it briefly further down.
3DBenchy, the test model every printer is judged by.Photo: Creative Tools ·CC BY 2.0 ·Wikimedia Commons
Printed Benchys in different filaments.Photo: 3DBenchy ·CC BY 2.0 ·Wikimedia Commons
The hull is a curved overhang test.Photo: CreativeTools: https://www.thingiverse.com/Cr… ·CC0 ·Wikimedia Commons
Benchy cut open: walls, infill and overhangs in one small boat.Photo: CreativeTools: https://www.thingiverse.com/Cr… ·CC0 ·Wikimedia Commons
Stringing on a two-colour Benchy, where travel moves cross open air.Photo: 3DBenchy ·CC BY 2.0 ·Wikimedia Commons
Strings and blobs across a full plate of parts.Photo: Quinn Daedal ·CC BY-SA 4.0 ·Wikimedia Commons
Another failed Benchy: messy, sagging layers.Photo: 3DBenchy ·CC BY 2.0 ·Wikimedia Commons
A twisted vase printed in a single wall.Photo: Sumanbargavr ·CC BY-SA 4.0 ·Wikimedia Commons
Why blobs and zits happen
When the printer pushes plastic into the hotend, it builds up pressure in the molten plastic inside the nozzle. That pressure is what pushes plastic out at a steady rate while the head moves. The trouble comes whenever the head stops, starts or slows down:
- When the head stops at the end of a wall, the pressure doesn’t vanish immediately, so a little more plastic oozes out. That leaves a bump.
- When the head starts again, it can take a moment for pressure to build, then overshoot. That can leave a bump or a small gap.
- During travel moves, hot plastic can drip from the nozzle and land on the wall when the nozzle arrives.
- At layer changes, the nozzle pauses while it moves up, and anything that oozes lands at the seam.
Every fix in this guide tackles one of these moments: reducing pressure before the stop (retraction, wipe, coasting, pressure advance), choosing where the stop happens (seam position), or reducing how much plastic is there to ooze in the first place (flow, temperature, dry filament).
retract 0.8 mm · 35 mm/s · 205 °C · strings: few
- drag ↔ retraction distance
- ← → retraction ±0.1 mm (Shift ±0.5)
- ↑ ↓ nozzle temperature ±5 °C
- − + retraction speed ±5 mm/s
- Space travel now
- Home reset
aligned · retract 0.8 mm · wipe off · PA off · bump medium
- S seam position: aligned · rear · nearest · random
- ← → retraction ±0.1 mm (Shift ±0.5), 0–2 mm; or drag ↔
- ↑ ↓ wipe ±0.5 mm, off–2 mm
- P pressure advance off / calibrated
- Home reset: aligned, 0.8 mm, no wipe, PA off
Cause and fix reference
| What you see | Most likely cause | Fix | Step |
|---|---|---|---|
| Zits stacked in a vertical line | Layer seam | Move or hide the seam | 1 |
| Zits where the nozzle stops or starts a wall | Ooze at the end and start of moves | Wipe, coasting, retraction tuning | 2 |
| Bulges at corners, thin spots after them | Pressure lag in the nozzle | Pressure advance | 3 |
| Zits scattered after travel moves | Ooze during travel | Avoid crossing walls, retraction | 4 |
| Lumpy walls everywhere, not just at stops | Too much plastic | Calibrate flow | 5 |
| Random zits, popping sounds, rough surface | Wet filament | Dry the spool | 6 |
| Zits on curved surfaces only | Printer stuttering on tiny segments | Arc fitting or lower G-code resolution | 7 |
| Large lumps landing on the print | Plastic collecting on the nozzle | Clean nozzle, check for leaks | Big blobs |
Step 1: Control the seam
Start here. Every outer wall loop has to start and end somewhere. That point is the seam, and it’s where most zits come from. You can’t remove it on a normal print, but you can choose where it goes.
Your slicer’s seam position setting usually offers some of these options:
- Aligned: every layer starts at the same spot. All the zits stack into one neat stripe. Good when that stripe can face away from view.
- Rear (or back): the seam is placed on the back of the part as it sits on the plate. Easy to hide: turn the model so its least visible side faces the back.
- Nearest: the seam goes wherever the nozzle happens to be closest. Fast, but the seam wanders and leaves zits across the surface.
- Random: the seam is placed at a different point each layer. There’s no stripe, but small zits are spread over the whole part.
- Sharpest corner (Cura’s “Hide or Expose Seam” corner preference does something similar): the slicer tucks the seam into an inside or outside corner, where it’s much harder to see.
For most parts, aligned or rear with the seam in a corner gives the cleanest result: all the zits in one line, tucked where you won’t notice them. On smooth round parts with no corners, choose between a single stripe at the back and random zits spread everywhere, depending on which bothers you less.
Some slicers (recent OrcaSlicer, Bambu Studio and PrusaSlicer versions) also offer a scarf seam option, which ramps the start and end of each loop up and down over a short distance instead of meeting at one point. It can make the seam almost disappear on round parts, at the cost of a little extra print time. Try it on a test cylinder first.11Scarf seams are newer and behave differently between slicers and versions.
If you use the seam painting tool in OrcaSlicer, Bambu Studio or PrusaSlicer, you can paint exactly where you want the seam to go, such as along a hidden edge.
A bed-slinger FDM printer halfway through a 225-layer print.
The finished part: 225 layers of 0.2 mm.
Useful prints: planters on a shelf.Photo: Aaaatu ·CC BY-SA 4.0 ·Wikimedia Commons
A printed bowl: walls only, no infill.Photo: Sumanbargavr ·CC BY-SA 4.0 ·Wikimedia Commons
A screw-top box: threads print well at 0.2 mm layers.Photo: syvwlch ·CC BY 2.0 ·Wikimedia Commons
A table of small prints.Photo: Trevor Prentice ·CC BY-SA 2.0 ·Wikimedia Commons
Step 2: Tune retraction, wipe and coasting
Retraction pulls the filament back a short distance before a travel move, so pressure in the nozzle drops and plastic doesn’t ooze. Get it wrong in either direction and you get zits.
- Too little retraction: plastic oozes during travel and lands on the wall, or forms a bump at the seam.
- Too much retraction, or a long “extra length on restart”: when the filament is pushed back in, a little too much comes out at once and leaves a blob at the start of the next wall.
- Retraction too slow: plastic keeps oozing during the retraction itself.
Typical starting ranges:
| Setting | Direct drive | Bowden | Why |
|---|---|---|---|
| Retraction distance | 0.5–2 mm | 4–7 mm | Bowden needs more because the long tube flexes and compresses |
| Retraction speed | 30–50 mm/s | 35–60 mm/s | Fast enough to drop pressure before the head moves |
| Extra length on restart (prime) | 0 mm | 0 mm | Extra priming is a common cause of start blobs |
| Minimum travel before retract | 1–2 mm | 1–2 mm | Avoids lots of tiny retractions that grind filament |
Change one value at a time, in small steps (0.2–0.5 mm on direct drive, 0.5–1 mm on Bowden). Too much retraction can pull molten plastic up into the cooler part of the hotend and cause clogs. Our guide to what retraction is explains the mechanism, and Bowden vs direct drive explains why the two setups need such different values.
Wipe
Wipe (sometimes “wipe while retracting”) moves the nozzle a short distance back along the wall it just printed while it retracts. Any plastic that oozes is smeared thinly onto the wall instead of left as a bump, and the nozzle leaves the surface clean. It’s one of the most effective fixes for seam zits.
- Start with a wipe distance of about 1–2 mm.
- In Cura, the closest setting is Outer Wall Wipe Distance, which moves the nozzle a little further after finishing the outer wall.
Coasting
Coasting (a Cura setting, in the Experimental section) stops pushing plastic shortly before the end of each wall and lets the remaining pressure in the nozzle finish the line. Done right, the line ends without a bump.
- Start small. Too much coasting leaves a gap or dent at the seam instead of a zit.
- Coasting and pressure advance both deal with leftover pressure. If you’ve calibrated pressure advance, you usually don’t need coasting, and using both can leave gaps.
A stringing test: two thin towers and a head that travels between them.
No retraction: many strings.
0.8 mm of retraction: a few strings.
The dial reads retraction in 0.25 mm steps.
Inside the hotend: solid filament above, melt below.
Too much retraction pulls melt up into the heat break.
Step 3: Calibrate pressure advance
Pressure advance (called linear advance in Marlin) is a firmware feature that adjusts extrusion ahead of speed changes. As the head slows into a corner or towards the end of a line, it eases off the extruder early so pressure drops in time. As the head speeds up, it pushes a little extra so pressure builds sooner.
Without it, you typically see:
- Bulging corners, with a thin or under-filled spot just after them.
- A zit at the seam where the line ends.
- Line ends that look thick and starts that look thin.
Pressure advance is available in Klipper, in Marlin (as linear advance, if it’s turned on in the firmware) and in Bambu Lab printers, where it’s calibrated automatically or through the slicer’s flow dynamics calibration.22The values aren’t interchangeable between firmwares or printers, so don’t copy a number from someone else’s setup. Run the calibration for your own printer and filament.
How to set it:
- Use your slicer’s built-in pressure advance calibration if it has one. OrcaSlicer has one under its Calibration menu, and Bambu Studio offers flow dynamics calibration.
- Otherwise, follow your firmware’s own guide: Klipper and Marlin both document a test print that steps through values.
- As a rough idea of scale, direct-drive printers tend to land somewhere around 0.02–0.1, and Bowden printers higher, around 0.3–1.0. The calibration is what decides the real value.
- Re-run it when you change filament type or brand, because each one flows differently.
If your printer doesn’t support pressure advance, wipe and careful retraction are your main tools for seam zits.
The print head: extruder on top, finned heatsink, heater block and nozzle.
A modern toolhead: extruder, hotend and fans in one housing.Photo: disinterpreter ·CC BY-SA 2.0 ·Wikimedia Commons
The toolhead rides the gantry; cable chains carry its wires.Photo: disinterpreter ·CC BY-SA 2.0 ·Wikimedia Commons
A geared extruder on a Prusa i3.Photo: John Abella from Outside Philadelphia, USA ·CC BY 2.0 ·Wikimedia Commons
An early Ultimaker extruder: a big gear pushing filament.Photo: jabella ·CC BY 2.0 ·Wikimedia Commons
An extruder motor with its tension knob.Photo: syvwlch ·CC BY 2.0 ·Wikimedia Commons
Step 4: Improve travel moves
Every time the nozzle crosses open air or the outer wall, it can drip a little plastic or drag a drop across the surface.
- Avoid crossing walls (OrcaSlicer, Bambu Studio, PrusaSlicer) or combing (Cura) keeps travel moves inside the part, so any ooze lands inside instead of on the visible surface. It adds a little travel time.
- Retract only when crossing perimeters (PrusaSlicer, and similar options elsewhere) saves retractions, but means the nozzle can ooze during travel inside the part. If zits appear on the surface near travel paths, turn it off.
- Wall printing order matters. Printing the inner walls first and the outer wall last (the default in most slicers) gives the best surface on the outside. When the outer wall is printed first, the nozzle has to travel inward right after the visible wall.
- Z hop lifts the nozzle during travel. It stops the nozzle dragging over the print, but it isn’t a cure for zits and can add a little stringing.
- Keep travel fast (150 mm/s or more on most modern printers) so there’s less time to ooze.
Heavy stringing across a detailed print.Photo: SuperBlobMonster ·CC BY-SA 3.0 ·Wikimedia Commons
Close up: strings stretched between every travel move.Photo: SuperBlobMonster ·CC BY-SA 3.0 ·Wikimedia Commons
A print head at work over a plate of small parts.Photo: Neon Tommy ·CC BY-SA 2.0 ·Wikimedia Commons
Step 5: Check for over-extrusion
If the printer pushes out more plastic than the slicer expects, the extra has to go somewhere. It builds up wherever the head slows down, and that’s at the seam and the corners.
How to recognise it:
- Walls look lumpy or rough all the way up, not only at the seam.
- Top surfaces have ridges and the nozzle drags through them.
- Parts measure larger than designed and holes come out too small.
The fix: calibrate the flow rate (also called extrusion multiplier), check the filament diameter setting matches your filament (usually 1.75 mm), and check the extruder steps are correct. Our guide to over-extrusion walks through each test. If you’re unsure what temperature your filament prints best at, a temperature tower is worth running too, because a nozzle that’s too hot makes plastic runnier and more likely to ooze.
| Filament | Typical nozzle range | Try first if you see zits |
|---|---|---|
| PLA | 190–220 °C | 200–205 °C |
| PETG | 220–250 °C | 230–235 °C |
| ABS / ASA | 230–260 °C | 240–245 °C |
| TPU | 210–235 °C | 215–220 °C, slow |
These are starting points, not targets. Stay within the range printed on your spool. PETG oozes most of the common filaments, so expect to tune it more than PLA; see PLA vs PETG and PLA vs ABS for how each material behaves.
A V6-style hotend, cut away so you can see the filament inside.
Solid filament above the heat break, molten filament in the heater block.
The heater block holds the heater cartridge and the thermistor.
Hotter plastic is runnier: thinner, saggier strings.
A heater block in a silicone sock, with the nozzle below and heat break above.Photo: A7N8X ·CC0 ·Wikimedia Commons
A hotend being built: the heater wrapped in Kapton tape.Photo: syvwlch ·CC BY 2.0 ·Wikimedia Commons
The nozzle threads into the heater block.Photo: syvwlch ·CC BY 2.0 ·Wikimedia Commons
The mount that holds the hotend to the carriage.Photo: syvwlch ·CC BY 2.0 ·Wikimedia Commons
Step 6: Dry your filament
Filament absorbs moisture from the air. When wet filament reaches the hot nozzle, the water turns to steam, which pushes out small bursts of extra plastic and leaves tiny bubbles. The result is random zits, a rough or fuzzy surface and extra stringing.
How to recognise it:
- Popping, crackling or hissing sounds while printing.
- Zits that appear randomly, not only at the seam or after travel.
- The problem got worse over time with the same spool and the same settings.
The fix: dry the spool, then store it sealed with desiccant. PETG, nylon and TPU are the most sensitive, but PLA can get wet too. Our guide to drying filament gives temperatures and times for each material.
An open spool of PLA left out in the air.Photo: SuperBlobMonster ·CC BY-SA 3.0 ·Wikimedia Commons
A 1 kg spool of PETG, sealed with desiccant.Photo: Suit ·CC BY-SA 4.0 ·Wikimedia Commons
A spool of white filament.Photo: Creative Tools ·CC BY 2.0 ·Wikimedia Commons
Read the label: material, 1.75 mm diameter, 1 kg.Photo: John Abella from Outside Philadelphia, USA ·CC BY 2.0 ·Wikimedia Commons
Step 7: Check firmware and arc settings
This cause is less common, but it’s worth knowing about if your zits appear only on curved surfaces.
Slicers describe curves as many short straight lines. On a detailed model, that can mean a huge number of tiny moves. If the printer can’t read and process them fast enough, especially when printing over a USB connection from a computer or an older print server, it briefly pauses between moves. Every pause lets the nozzle ooze, leaving small zits along curves.
Fixes to try:
- Arc fitting (OrcaSlicer, Bambu Studio, PrusaSlicer) replaces runs of short lines with smooth arc commands (G2/G3), so there are far fewer moves. Your firmware has to support arc commands: in Marlin this is an option that must be turned on when the firmware is built, and in Klipper it needs a
[gcode_arcs]section in the config. If you’re not sure, check your printer’s documentation before turning it on. - Lower the G-code resolution. In Cura, the Maximum Resolution and Maximum Deviation settings control how finely curves are split; the defaults are usually fine, and very small values create many more tiny moves.
- Print from the SD card or the printer’s own storage instead of streaming over USB, if your setup allows it. If your printer runs Klipper or a recent Bambu Lab firmware and you print from its own storage, this is unlikely to be your cause.
Big blobs that fall off the nozzle
Sometimes a much larger lump lands on the print: plastic that has slowly collected on the outside of the nozzle and then drops off. This isn’t the same as a zit, but it’s often searched for under the same name.
- Clean the nozzle while it’s hot with a brass brush, carefully.
- Fit a silicone sock on the heater block if your hotend takes one. Plastic sticks to silicone far less than to bare metal.
- Check the first layer. A nozzle that’s too close to the bed digs into the plastic and picks it up. See what is Z offset.
- Check for leaks. If plastic is coming out from between the nozzle and the heater block, the nozzle wasn’t tightened properly against the heat break. That needs to be fixed hot, following your printer’s instructions. Our guide to unclogging a nozzle covers nozzle care.
The extreme version is the “blob of death”: a print comes loose or a nozzle leaks, and molten plastic wraps the whole heater block. That’s a hardware rescue job, not a print-quality setting.
The "blob of death": plastic that leaked and wrapped the hotend.Photo: LunaEatsTuna ·CC BY-SA 4.0 ·Wikimedia Commons
A "spaghetti monster": what a failed print looks like after hours of printing into nothing.Photo: A7N8X ·CC0 ·Wikimedia Commons
Fan off: heat creeps up the heatsink and the filament softens too high.
Where to find these settings in your slicer
| Setting | OrcaSlicer / Bambu Studio | PrusaSlicer | Cura |
|---|---|---|---|
| Seam position | Process → Quality → Seam position | Print Settings → Layers and perimeters → Seam position | Walls → Z Seam Alignment |
| Wipe | Wipe while retracting / Wipe distance (printer or filament retraction settings) | Printer Settings → Extruder → Wipe while retracting | Outer Wall Wipe Distance |
| Coasting | Not a standard setting | Not a standard setting | Experimental → Enable Coasting |
| Retraction | Printer settings → Extruder (filament can override) | Printer Settings → Extruder → Retraction | Travel → Retraction Distance |
| Avoid crossing walls | Avoid crossing walls | Avoid crossing perimeters | Combing Mode |
| Pressure advance | Pressure advance option in filament settings, plus the Calibration menu | Set in printer firmware or start G-code | Set in printer firmware or start G-code |
| Arc fitting | Arc fitting | Arc fitting | Not built in; Maximum Resolution controls segment length |
Menu names move between slicer versions. If you can’t find a setting, type its name into the slicer’s settings search box. Our guide to using a slicer explains the difference between process, filament and printer settings.
When the zits won’t go away
- Reset to the stock profile for your printer and filament, then change one thing at a time. Several half-tuned settings can work against each other.
- Check you’re not stacking fixes. Coasting, wipe, long retraction and pressure advance all reduce pressure at the end of a line. Too many together leave gaps at the seam.
- Try a different spool. If a fresh spool prints cleanly, the old one is wet or poor quality.
- Check for a partial clog. An extruder that clicks or skips can surge and leave uneven lines. See extruder clicking and under-extrusion.
- Accept a tidy seam. A thin, straight line at the back is a good result on any print that isn’t in vase mode.
A working wrench printed in one piece.Photo: Creative Tools from Halmdstad, Sweden ·CC BY 2.0 ·Wikimedia Commons
A printed maze puzzle.Photo: Sumanbargavr ·CC BY-SA 4.0 ·Wikimedia Commons
Test prints on the way from failure to a clean part.Photo: Dbsnp ·CC BY-SA 4.0 ·Wikimedia Commons
A two-colour Benchy.Photo: 3DBenchy ·CC BY 2.0 ·Wikimedia Commons
FAQ
What causes zits on 3D prints?
Extra plastic left where the nozzle stops, starts or slows down. The most common places are the layer seam, the end of a retraction and the end of a travel move. Wet filament, over-extrusion and a nozzle that’s too hot make it worse.
How do I get rid of the Z seam?
You can’t remove it on a normal print, because every layer has to start somewhere. You can hide it: set the seam to rear or aligned and tuck it into a corner, or paint it onto a hidden edge. Wipe, pressure advance and scarf seams make the seam itself smaller. Vase mode prints a single continuous spiral, so it has no seam at all.
Does retraction cause blobs?
It can. Too little retraction lets plastic ooze; too much, or extra priming on restart, pushes out a blob when printing resumes. Keep retraction in the normal range for your extruder type and set any extra restart length to 0.
What is pressure advance and do I need it?
Pressure advance adjusts the extruder ahead of speed changes so the nozzle pressure matches the head’s speed. It reduces bulging corners and seam zits. You don’t strictly need it, but it’s one of the most effective fixes if your firmware supports it.
What’s the difference between stringing and zits?
They come from the same oozing. Stringing happens when the ooze is pulled into thin threads during travel moves. Zits happen when the ooze is left on the wall where the nozzle stops or starts. Fixes like retraction, lower temperature and dry filament help both.
Related guides
Zits share their causes with stringing and over-extrusion, so check those next. To understand the main fix, read what is retraction. If walls show wavy patterns rather than bumps, see ringing and ghosting. New to printing? Start with the complete beginner’s guide.