Temperature Tower: How to Find the Best Print Temperature
What a temperature tower is, how to make one in OrcaSlicer, Bambu Studio, PrusaSlicer or Cura, and how to read it to pick the best nozzle temperature.
A temperature tower is a single test print made of stacked sections, each printed at a different nozzle temperature, usually 5 °C apart. You compare the sections for stringing, overhangs, bridges, layer strength and surface finish, then use the coolest temperature that still prints strong, clean layers.
This guide explains why the right temperature matters, how to generate a tower in OrcaSlicer, Bambu Studio, PrusaSlicer and Cura, how to read the result section by section, and which ranges to test for each common material. It works on any FDM printer.
Quick checklist
- Dry the filament first if it’s been sitting out. Wet filament ruins the test.
- Choose a range that covers the label on your spool, with 5–10 °C extra at each end.
- Generate the tower: built in to OrcaSlicer and Bambu Studio; with a downloaded model and per-height temperature changes in PrusaSlicer or Cura.
- Print it with your normal settings for speed, cooling and retraction, so the result matches your real prints.
- Judge each section for stringing, bridges, overhangs, surface and layer strength.
- Pick the coolest section that’s strong and clean, then add up to 5 °C for parts that need extra strength.
- Save the temperature in your filament profile so you never have to remember it.
Why print temperature matters
Every filament has a window where it melts properly, flows smoothly and bonds to the layer below. The spool label gives you that window, for example 190–220 °C for PLA. But where your sweet spot sits inside it depends on things the filament maker can’t know:
- Your printer’s thermistor. Temperature sensors read slightly differently from printer to printer, so “210 °C” on one machine isn’t exactly 210 °C on another.11A thermistor is a small sensor in the heater block that tells the printer how hot it is. Small differences in sensor, wiring and placement mean the displayed temperature can be a few degrees off the real one.
- Your print speed. Faster printing pushes more plastic through the hotend each second, which gives it less time to heat up. Fast printers usually need a hotter nozzle than slow ones.
- Your nozzle. Hardened steel nozzles conduct heat less well than brass, so they often need 5–10 °C more.
- The exact spool. Brands, and even colours from the same brand, flow differently because of their pigments and additives.
Getting the temperature wrong shows up in predictable ways:
| Too hot | Too cold |
|---|---|
| Stringing and oozing | Weak layers that split apart |
| Saggy overhangs and bridges | Rough, matte or gappy surfaces |
| Glossy, blobby, soft-looking surfaces | Under-extrusion and thin walls |
| Fine details melt together | Extruder clicking as it struggles to push |
| More heat creep and clog risk on long prints | Poor first-layer grip on some materials |
A temperature tower shows all of these side by side on one print, so you can see where your filament stops being too cold and starts being too hot.
195 °C, 0.8 mm retraction: few strings.
210 °C, 0.8 mm retraction: few strings.
225 °C, 0.8 mm retraction: many strings.
What a temperature tower looks like
Most temperature tower models share the same layout. The tower is split into stacked blocks, often around 10 mm tall each, and each block is printed at a different temperature. A typical block includes:
- A label with the temperature, so you know which block is which.
- An overhang: a face that leans out at an angle, often 45° or steeper, to show sagging and curling.
- A bridge: a short span of plastic printed across open air between two supports.
- Small spikes or cones, or a gap the nozzle travels across, to show stringing.
- Flat walls to judge the surface finish.
Most towers print hottest at the bottom and coolest at the top. Cooler plastic on top of a hotter, well-bonded base prints more reliably than the other way round, and the tower stays stable even if the cold sections are weak.
210 °C · 1 string · overhang sag 0.2 mm · bridge droop 0.2 mm · satin · layers 99 % · good
- ↑ ↓ next block up (cooler) or down (hotter); or click a block
- Home End bottom (230 °C) or top (190 °C)
- B the pick: the coolest strong, clean block (205 °C here)
How to make a temperature tower
Before you start
- Dry the spool if it’s been out of a sealed box for a while. Wet filament strings and bubbles at every temperature, which hides what the tower is trying to show you. See how to dry filament.
- Choose the right filament profile in your slicer. The tower uses its cooling, speed and retraction settings, so they should match what you’ll print with.
- Get your first layer right. A tower that comes loose halfway up wastes the test. If prints struggle to stick, sort that first with first layer not sticking.
OrcaSlicer
OrcaSlicer has a temperature tower built in.
- Select your printer and the filament profile you want to test.
- Open the Calibration menu in the top bar and choose Temperature.
- Pick the filament type, then set a start temperature and end temperature. The tower prints from the start (bottom) to the end (top) in 5 °C steps.
- OrcaSlicer creates a new project with the tower and the temperature changes already set. Slice and print it.
The blocks are labelled with their temperatures, so there’s nothing to write down.
Bambu Studio
Bambu Studio offers a similar set of calibration tests, including a temperature test, through its Calibration options. Select your printer and filament first, choose the temperature test, enter the start and end temperatures, and it generates the tower for you.
Menu names and layouts move between slicer versions. If you can’t find the option, look for “Calibration” in the top menus or search the slicer’s help for “temperature”.
PrusaSlicer
PrusaSlicer doesn’t generate a temperature tower for you, so you use a downloaded model and add the temperature changes yourself.
- Download a temperature tower model from a site like Printables. Note how tall each block is and which temperature each one is meant for; the model’s description usually says.
- Slice it with your normal filament profile, and set the starting nozzle temperature to the bottom block’s value.
- Switch to the Preview and use the vertical layer slider to move to the first layer of the second block.
- Click the plus icon next to the slider to add a change at that layer, and choose to add custom G-code (right-clicking the plus icon offers this option). Enter a temperature command such as
M104 S225. - Repeat at the start of every block, stepping the temperature down each time.
- Slice again and print.22
M104 S225tells the printer “set the nozzle to 225 °C and keep printing”. The printer reaches the new temperature over the next few layers, so the first millimetre or so of each block is a blend of the old and new temperature.
Cura
Cura also needs a downloaded model plus temperature changes at set heights.
- Download a temperature tower model and check the block heights in its description.
- Open Extensions → Post Processing → Modify G-Code.
- Add a script called ChangeAtZ (Change At Z). Set the height or layer where the second block starts, tick the option to change the extruder temperature, and enter the new value.
- Add one ChangeAtZ script for each block.
- Slice and print.
Cura’s Marketplace also has community plugins that generate calibration towers automatically. If you test filaments often, one of these saves time.
A 20 mm calibration cube, often the first print.Photo: syvwlch ·CC BY 2.0 ·Wikimedia Commons
The first layers going down on a heated bed.Photo: syvwlch ·CC BY 2.0 ·Wikimedia Commons
A print head at work over a plate of small parts.Photo: Neon Tommy ·CC BY-SA 2.0 ·Wikimedia Commons
Choosing the temperature range
Cover the range on your spool’s label, plus a little extra at each end, in 5 °C steps. Going slightly beyond the label shows you clearly where the filament fails, which makes it easier to judge the sections in between.
| Material | Typical tower range | Most people land around | Notes |
|---|---|---|---|
| PLA | 230 → 190 °C | 200–215 °C | Faster printers often land at the higher end |
| PLA+ / tough PLA | 235 → 200 °C | 210–225 °C | Varies a lot between brands |
| Silk PLA | 235 → 200 °C | 210–225 °C | Often a little hotter than plain PLA for shine |
| PETG | 255 → 220 °C | 230–245 °C | Strings more at the top of its range |
| ABS | 265 → 230 °C | 240–255 °C | Print in an enclosure, or the tower may crack |
| ASA | 265 → 235 °C | 245–260 °C | Same as ABS: enclosure recommended |
| TPU (95A) | 240 → 210 °C | 220–235 °C | Print slowly; many towers are fine at low speed |
| Nylon | 280 → 240 °C | 250–270 °C | Must be bone dry; needs an all-metal hotend |
These are starting points to centre your tower on, not answers. The point of the test is to find your number. For more on each material, see the filament guide.
How to read a temperature tower
Let the tower cool fully, then look at it in good light, turning it so light grazes across the surface. Judge the middle of each block, not the first millimetre or two, because the printer takes a few layers to settle at each new temperature.
Work through these five checks.
1. Stringing
Look at the spikes, cones or gaps between features. Hotter blocks usually have more and thinner strings, because the plastic is runnier and oozes during travel moves. As the temperature drops, the strings should thin out and then disappear.
Some stringing at every temperature usually means wet filament or not enough retraction rather than the wrong temperature. Dry the spool, then see how to fix stringing and what is retraction.
Close up: strings stretched between every travel move.Photo: SuperBlobMonster ·CC BY-SA 3.0 ·Wikimedia Commons
A thin strand pulled from the nozzle: where strings begin.Photo: David Elliott from UK ·CC BY 2.0 ·Wikimedia Commons
0.8 mm of retraction: a few strings.
2. Bridges
Look at the underside of each bridge. A good bridge is fairly flat, with lines that are straight and touch each other. When the plastic is too hot, it stays soft for longer and the bridge sags or droops in the middle. Too cold, and lines can break or look stringy and thin.
Bridges also depend heavily on cooling, so if every block’s bridge sags, check your part cooling fan before blaming temperature.
3. Overhangs
Look at the angled faces. Hot plastic curls up at the edges and leaves a rough, droopy underside, because each new line sits on soft plastic that hasn’t set yet. Cooler blocks usually give cleaner, sharper overhangs, up to the point where layers stop bonding.
4. Surface finish
Look at the flat walls and the labels:
- Too hot: glossy, slightly blobby walls, soft edges, numbers that look melted.
- About right: even, consistent walls with clean edges and readable labels.
- Too cold: matte or rough walls, visible gaps between lines, and sometimes missing bits of plastic. That’s under-extrusion caused by plastic that can’t flow fast enough.
Some filaments change colour or gloss with temperature, especially silk and matte blends. Choose the look you prefer as long as it passes the strength check.
5. Layer strength
This is the check most people skip, and the most important for functional parts. A block can look perfect and still be weak.
Once you’ve looked at everything else, try to break the tower. Grip it above and below each block and bend it, or snap each block off with pliers. Notice where it breaks and how:
- Strong layers take real effort to break, and the break is jagged and doesn’t follow the layer lines cleanly.
- Weak layers split cleanly along a layer line with little effort.
Cold blocks almost always break more easily. Write down the lowest temperature where layers still feel strong.
Picking your temperature
Put the five checks together:
- Rule out the hot blocks with obvious stringing, saggy bridges and curled overhangs.
- Rule out the cold blocks with weak layers, rough walls or gaps.
- Of what’s left, pick the coolest block that still has strong layers and a clean surface. Cooler printing gives the least stringing and the sharpest detail.
- For parts that need strength, consider using 5 °C above that. You trade a little stringing for better layer bonding.
If two neighbouring blocks look equally good, choose the one in between them, or the cooler one for decorative prints and the warmer one for functional parts.
Then save it in your filament profile, not just for this one print. In most slicers, edit the filament’s nozzle temperature and save it as a new profile named after the brand and colour, such as “Brand X PLA white”. The next time you load that spool, it’s already right. Our slicer guide covers creating and saving profiles.
190 °C, 0.8 mm retraction: no strings.
200 °C, 0.8 mm retraction: few strings.
215 °C, 0.8 mm retraction: some strings.
230 °C, 0.8 mm retraction: many strings.
Tips and common mistakes
| Mistake | What goes wrong | Do this instead |
|---|---|---|
| Testing wet filament | Strings and bubbles at every temperature | Dry the spool first |
| Printing the tower at a different speed from your real prints | The best temperature shifts with speed | Use your normal print profile |
| Judging the first layers of each block | Those layers are still changing temperature | Judge the middle of each block |
| Looking but not breaking | A good-looking block may have weak layers | Always do the snap test for functional parts |
| One tower per material, forever | Brands and colours differ | Run a quick tower for each new brand or unusual colour |
| Testing ABS or ASA in open air | Tall, thin towers crack and warp | Use an enclosure, or test with a brim |
| Ignoring the fan | Bridges and overhangs depend on cooling as much as heat | Keep cooling at your normal setting during the test |
ABS, bed 100 °C, open air: ABS · bed 100 °C · open air · corner lift 0.80 mm · warping.
ABS enclosed, with a brim: ABS · bed 100 °C · enclosed · brim · corner lift 0.00 mm · flat.
An enclosure keeps heat in for ABS and ASA.Photo: -stk ·CC BY-SA 4.0 ·Wikimedia Commons
What to calibrate next
The temperature tower comes first because temperature affects almost everything else. Once you’ve picked your temperature, these are the usual next steps:
- Retraction. With the temperature settled, tune retraction to clear up any remaining strings. See what is retraction and how to fix stringing.
- Flow. If walls look too thin or top surfaces look ridged and overfull, adjust flow. See under-extrusion and over-extrusion.
- Speed and acceleration. If you see ripples after sharp corners, read ringing and ghosting.
If the tower kept failing for mechanical reasons, such as layers shifting sideways or the extruder clicking, fix those first: see layer shifting and extruder clicking.
retract 0.8 mm · 35 mm/s · 205 °C · strings: few
- drag ↔ retraction distance
- ← → retraction ±0.1 mm (Shift ±0.5)
- ↑ ↓ nozzle temperature ±5 °C
- − + retraction speed ±5 mm/s
- Space travel now
- Home reset
Solid filament above the heat break, molten filament in the heater block.
Inside the hotend: solid filament above, melt below.
The heater block holds the heater cartridge and the thermistor.
Fan off: heat creeps up the heatsink and the filament softens too high.
FAQ
What is a temperature tower in 3D printing?
A test print built from stacked sections, each printed at a different nozzle temperature. Comparing the sections shows which temperature gives the best balance of strength, surface quality and stringing for your filament and printer.
How many degrees apart should each section be?
5 °C is the usual step. It’s small enough to find a precise answer and large enough that you can see the difference between sections. 10 °C steps are fine for a quick first look across a wide range.
Should a temperature tower start hot or cold?
Most towers print hottest at the bottom and coolest at the top. Cold sections can be weak, and you don’t want weak sections holding up the rest of the tower.
Do I need a new temperature tower for every spool?
Not for every spool of the same filament. Do run one for each new brand, each new material, and unusual colours like silk, glow or very dark pigments, which can flow differently.
Does print speed change the best temperature?
Yes. Faster printing pushes more plastic through the hotend, giving it less time to heat, so fast printers usually need a hotter nozzle. Print the tower at the speed you normally use.
Can a temperature tower fix stringing?
It often helps, because printing cooler reduces ooze. But if every section strings, the cause is more likely wet filament or retraction settings. Dry the spool and tune retraction next.
Does PrusaSlicer have a built-in temperature tower?
Not in the same way as OrcaSlicer. In PrusaSlicer you download a tower model and add temperature changes at each block using the layer slider in the preview.
Why does my tower look good but snap easily?
The temperature is likely too low for good layer bonding, even though the surface looks clean. Use a slightly hotter block from the tower for parts that need strength.
Related guides
- Choose the right material first: the 3D printing filament guide and PLA vs PETG.
- Clean up what the tower reveals: how to fix stringing and under-extrusion.
- New to all this? Start with the complete beginner’s guide.