Nozzle School · Troubleshooting
Elephant's Foot in 3D Printing: Causes and Fixes
Why the bottom layers of a 3D print bulge outwards and how to fix it: Z offset, bed temperature, first-layer flow, cooling and elephant foot compensation.
Elephant’s foot is a bulge or lip around the bottom few layers of a 3D print, where they spread wider than the rest of the part. It’s caused by too much squish and heat at the bottom: the nozzle is too close to the bed, the bed is too hot, or the first layer gets too much plastic. You fix it by raising the Z offset slightly, lowering the bed temperature, and then using your slicer’s elephant foot compensation to trim the last bit.
This guide covers every common cause, how to tell them apart, and where to find the settings in OrcaSlicer, Bambu Studio, PrusaSlicer and Cura. It works on any FDM printer.
Quick fix checklist
Work down this list and re-print a small test (a 20 mm cube is ideal) after each change:
- Raise the Z offset by 0.02–0.05 mm if your first layer looks shiny, flattened and wide.
- Lower the bed temperature by 5 °C at a time, staying inside your filament’s range.
- Check first-layer flow and line width aren’t set higher than the rest of the print.
- Turn the part-cooling fan on sooner, from layer 2 or 3 instead of much later.
- Re-level the bed if the bulge is worse on one side than the other.
- Turn on elephant foot compensation, starting at 0.1–0.2 mm.
- Add a small chamfer to the bottom edge of parts you design yourself.
Too low: lines squashed thin, and the extruder struggles.
Z offset right: slightly squished lines that touch.
Too high: round lines that don't touch or stick.
A 20 mm calibration cube, often the first print.Photo: syvwlch ·CC BY 2.0 ·Wikimedia Commons
The calibration cube a few layers in.Photo: syvwlch ·CC BY 2.0 ·Wikimedia Commons
A first layer close up: lines pressed together on the bed.Photo: hdaniel ·CC BY-SA 2.0 ·Wikimedia Commons
What is elephant’s foot?
Elephant’s foot (sometimes written “elephant foot”) is the name for the bottom layers of a print flaring outwards, like the base of an elephant’s leg. Look at the bottom edge of a box or cube from the side: instead of a straight wall, you see a lip that sticks out a fraction of a millimetre, usually over the first 2–5 layers.
It’s mostly a cosmetic and fit problem. A small lip doesn’t weaken the part, but it makes the base bigger than you designed it, so boxes don’t sit flat against each other, lids and holes at the bottom are too tight, and parts that should slot together won’t.
Elephant’s foot and faults that look similar
- Elephant’s foot: only the bottom few layers bulge outwards; everything above is straight.
- First layer too squished: the first layer is flat, shiny and see-through in places, sometimes with ridges. It’s the most common cause of elephant’s foot, and you fix it the same way.
- Over-extrusion: too much plastic on every layer, not just the bottom. Walls look lumpy all the way up and dimensions are oversized everywhere.
- Warping: the corners lift off the bed. It’s the opposite problem, and the fixes for warping (hotter bed, closer nozzle) can push you towards elephant’s foot if you overdo them.
- Brim left behind: a thin ring of plastic around the base after you peeled off a brim. That’s a brim removal problem, not a bulge in the part.
Cross-section, too low: the line is pressed into a sheet.
Cross-section, right height: a flattened line, about 0.45 × 0.20 mm.
Cross-section, too high: the line stays round.
Nozzle height decides the first layer: too close, just right, too far.Photo: Stemfie3D ·CC BY-SA 4.0 ·Wikimedia Commons
ABS, bed 100 °C, open air: ABS · bed 100 °C · open air · corner lift 0.80 mm · warping.
PLA, bed 60 °C: PLA · bed 60 °C · open air · corner lift 0.00 mm · flat.
Test prints on the way from failure to a clean part.Photo: Dbsnp ·CC BY-SA 4.0 ·Wikimedia Commons
The first layers going down on a heated bed.Photo: syvwlch ·CC BY 2.0 ·Wikimedia Commons
Why elephant’s foot happens
Your slicer asks for a first layer of a certain size, usually about 0.2 mm high and 0.4–0.5 mm wide. If the nozzle is closer to the bed than the slicer expects, the same amount of plastic has to go somewhere, so it spreads sideways. The outer wall of the first layer ends up wider than the walls above it.
Heat makes it worse. The heated bed keeps the bottom layers warm, and if they stay near or above the filament’s glass transition temperature (the point where it goes from hard to rubbery, about 60 °C for PLA) they stay soft. Each new layer presses down on them as it’s printed, and the soft bottom slowly squashes outwards under the weight and pressure.
So elephant’s foot comes down to three things: how much the first layers are squished (Z offset and flow), how soft they stay (bed temperature and cooling), and whether the slicer corrects for it (elephant foot compensation).
base 1.10 vs wall 0.90 mm · slight lip · gap 0.20 · bed 60 °C · flow 100 % · fan L3 · comp 0.00
- ↑ ↓ nozzle gap (Z offset) ±0.02 mm, 0.10–0.30; or drag ↕
- ← → bed temperature ±5 °C, 40–80 °C (or click the controller)
- F first-layer flow +5 %, 90–120 % (Shift −; or click the wall)
- 1–6 layer the part-cooling fan turns on (or click the blower)
- C elephant foot compensation +0.05 mm, 0–0.3 (Shift −; or click the caliper)
- Home reset: gap 0.20, bed 60 °C, flow 100 %, fan from layer 3, no compensation
gap 0.20 mm · line 0.45 × 0.20 mm · good squish
- Drag ↕ raise / lower the nozzle
- ↑ ↓ one babystep, 0.02 mm (Shift: 0.10)
- 1 2 3 too high · good · too low
- Home back to 0.00
Z offset −0.10 mm: gap 0.10 mm · line 0.84 × 0.10 mm · too low · lines pile into ridges.
Z offset −0.06 mm: gap 0.14 mm · line 0.61 × 0.14 mm · good squish.
Z offset −0.02 mm: gap 0.18 mm · line 0.49 × 0.18 mm · good squish.
Z offset 0.00 mm: gap 0.20 mm · line 0.45 × 0.20 mm · good squish.
Z offset +0.02 mm: gap 0.22 mm · line 0.42 × 0.22 mm · good squish.
Z offset +0.04 mm: gap 0.24 mm · line 0.39 × 0.24 mm · too high · gaps between lines.
Z offset +0.08 mm: gap 0.28 mm · line 0.35 × 0.28 mm · too high · gaps between lines.
Z offset +0.12 mm: gap 0.32 mm · line 0.32 × 0.32 mm · too high · gaps between lines.
Cause and fix reference
| What you see | Most likely cause | Fix | Step |
|---|---|---|---|
| Shiny, flat first layer with ridges; lip on every side | Nozzle too close | Raise Z offset | 1 |
| Bulge grows over several layers, worse on tall or heavy parts | Bed too hot | Lower bed temperature | 2 |
| Lip appears even with a good Z offset | Too much first-layer flow or width | Reset first-layer flow and line width | 3 |
| Bottom layers stay soft and glossy for a while after printing | Fan off for too many layers | Turn cooling on sooner | 4 |
| Bulge on one side or one corner only | Bed not level | Re-level or re-probe the bed | 5 |
| A small, even lip remains after all of the above | Normal first-layer squish | Elephant foot compensation | 6 |
| Parts you design must fit exactly at the base | Any remaining lip | Chamfer the bottom edge | 7 |
Step 1: Check the Z offset
Start here. A nozzle that’s too close to the bed is the most common cause of elephant’s foot. With too small a gap, the first layer is pressed flat and wide, and the outer wall gets pushed out past where it should be.
How to recognise it:
- The first layer looks glossy and very flat, sometimes almost see-through.
- You see small ridges where lines have piled into each other.
- The extruder may click or skip on the first layer, because there’s nowhere for the plastic to go. Our guide to why an extruder clicks covers that symptom.
The fix: raise the nozzle in 0.02–0.05 mm steps while a large single-layer square prints, until the lines are slightly flattened and just touch each other. Small steps matter because the whole first layer is only about 0.2 mm thick, so 0.05 mm is a quarter of it. Our guide to Z offset shows how to adjust it live on every common type of printer.
Z offset −0.12 mm: gap 0.08 mm · line 0.54 × 0.08 mm · too low · extruder skipping.
Z offset −0.08 mm: gap 0.12 mm · line 0.70 × 0.12 mm · too low · lines pile into ridges.
Z offset −0.04 mm: gap 0.16 mm · line 0.54 × 0.16 mm · good squish.
Z offset +0.06 mm: gap 0.26 mm · line 0.37 × 0.26 mm · too high · gaps between lines.
Z offset +0.10 mm: gap 0.30 mm · line 0.34 × 0.30 mm · too high · gaps between lines.
Z offset +0.14 mm: gap 0.34 mm · line 0.32 × 0.32 mm · too high · round strand, won't stick.
Each click of the babystep wheel moves the nozzle 0.02 mm.
Too low, the pressure rises until the extruder skips.
A 0.20 mm feeler leaf: the gap for a standard first layer.
A touch probe sits beside the nozzle and taps the bed.
A print bed in layers: heater, aluminium, magnet, spring steel, PEI.
Step 2: Lower the bed temperature
A hot bed helps the first layer stick, but it also keeps the bottom layers soft. If they stay above the plastic’s glass transition, the weight of the layers above and the pressure of the nozzle on every new layer slowly squash them outwards. The taller and heavier the part, the more this shows.
How to recognise it: the bulge spreads over several layers rather than just the first one, and it’s worse on large or tall parts than on small ones.
The fix: lower the bed temperature in 5 °C steps, staying inside your filament’s recommended range. The goal is the coolest bed that still holds the part firmly to the end of the print.
| Filament | Typical bed range | Try first if you see elephant’s foot |
|---|---|---|
| PLA | 50–65 °C | 50–55 °C |
| PETG | 70–85 °C | 70–75 °C |
| ABS / ASA | 90–110 °C | 90–100 °C, in an enclosure |
| TPU | 30–60 °C | 40 °C or lower |
PLA is the most sensitive, because its glass transition (about 60 °C) sits right inside its usual bed range.11Many printer profiles use a hotter bed for the first layer than for the rest of the print. Lowering only the “other layers” temperature, and leaving the first layer a little warmer, keeps adhesion while letting the base firm up sooner. Our PLA vs PETG guide covers the typical temperatures for each.
The bed controller: actual temperature, setpoint and material.
PLA, bed 60 °C: PLA · bed 60 °C · open air · corner lift 0.00 mm · flat.
PLA on a cold bed: PLA · bed 20 °C · open air · corner lift 0.62 mm · warping.
The heated bed with a PEI sheet. The part is the only thing printed on it.
A part being printed on a spring-steel bed.Photo: Leonhard Lenz ·CC BY-SA 4.0 ·Wikimedia Commons
A print on a glass bed.Photo: ENERGY.GOV ·Public domain ·Wikimedia Commons
Step 3: Check first-layer flow and line width
Even with a perfect Z offset, the first layer can be given more plastic than it needs. Many slicer profiles deliberately print the first layer wider, or with extra flow, to help it stick. A little is fine; too much and the outer wall spreads out.
How to recognise it: the first layer looks over-full even when the Z offset tests well, or the lip appeared after you changed profiles or copied settings from another printer.
What to check:
- First-layer line width: 100–125 % of the nozzle size is typical (0.4–0.5 mm on a 0.4 mm nozzle). Wider lines push more plastic outwards.
- First-layer flow: keep it at 100 % unless you have a reason not to. If it’s been raised, bring it back down.
- Overall flow rate: if every layer is oversized, not just the bottom, the problem is general over-extrusion. Calibrate flow first, then come back to the first layer.
- First-layer nozzle temperature: a profile 5–10 °C hotter for the first layer is common. If yours is much hotter than that, the plastic stays runnier and spreads more.
A brass 0.4 mm nozzle laying a thin strand.
Molten plastic leaving the nozzle.Photo: David Elliott from UK ·CC BY 2.0 ·Wikimedia Commons
Feed 2 mm/s: nozzle 210 °C · heatsink 38 °C · feed 2.0 mm/s · melting in block.
Feed 4 mm/s: nozzle 210 °C · heatsink 38 °C · feed 4.0 mm/s · melting in block.
A geared extruder on a Prusa i3.Photo: John Abella from Outside Philadelphia, USA ·CC BY 2.0 ·Wikimedia Commons
An extruder motor with its tension knob.Photo: syvwlch ·CC BY 2.0 ·Wikimedia Commons
The print head: extruder on top, finned heatsink, heater block and nozzle.
Read the label: material, 1.75 mm diameter, 1 kg.Photo: John Abella from Outside Philadelphia, USA ·CC BY 2.0 ·Wikimedia Commons
Step 4: Cool the bottom layers sooner
Most profiles turn the part-cooling fan off for the first layer or two, so the plastic stays warm and sticks. If the fan stays off for many layers, or ramps up very slowly, the bottom of the print stays soft for longer and sags under the layers above.
The fix: keep the fan off for the first 1–3 layers, then let it come on. For PLA, full fan from about layer 3 onward is normal. PETG usually prints with less fan (around 30–50 %), and ABS or ASA with little or none, so for those materials lean on bed temperature and compensation instead.22Turning the fan on for the very first layer usually hurts adhesion more than it helps the bulge, so most profiles leave it off there.
The hotend fan cools the heatsink. It must run whenever the hotend is hot.
A small fan cooling the extruder assembly.Photo: syvwlch ·CC BY 2.0 ·Wikimedia Commons
A print head at work over a plate of small parts.Photo: Neon Tommy ·CC BY-SA 2.0 ·Wikimedia Commons
Step 5: Level the bed
If elephant’s foot is worse on one side or one corner of the part, the gap between nozzle and bed isn’t the same everywhere. That corner is effectively printing with a lower Z offset than the rest.
The fix: re-level the bed or re-run your printer’s automatic bed leveling, then check the Z offset again. A probe mesh only matches the bed it measured, so probe again after you’ve turned any knobs or swapped the build plate. Our guide to leveling your bed covers manual and automatic leveling step by step.
mesh 25/25 · range 0.29 mm · corner FL +0.12 mm
- 1–4 pick a corner: FL, FR, BR, BL (or click its knob)
- ← → turn its knob ⅛ turn, 0.06 mm (Shift: ½ turn)
- drag ↔ turn the picked knob
- P probe the 5 × 5 mesh
- Space print a first-layer test
- Home reset
A probed 5 × 5 mesh across the bed.
The mesh: 25 measured heights the printer follows on the first layer.
Turn a knob and the old mesh no longer matches the bed. Probe again.
A corner spring and knob: about half a millimetre per full turn.
Front left knob turned −½ turn (about 0.25 mm): corner FL −0.13 mm · ¼ turn low · mesh out of date.
Front left knob turned −¼ turn (about 0.13 mm): corner FL +0.00 mm · level · mesh out of date.
Front left knob turned +¼ turn (about 0.13 mm): corner FL +0.25 mm · ½ turn high · mesh out of date.
Front left knob turned +½ turn (about 0.25 mm): corner FL +0.37 mm · ¾ turn high · mesh out of date.
Step 6: Use elephant foot compensation
Some squish on the first layer is needed for it to stick, so even a well-tuned printer can leave a tiny lip. Slicers handle this with elephant foot compensation: they shrink the outline of the first layer (or first few) inward by a set amount, so that after it’s squished it ends up the right size.
- Start at 0.1–0.2 mm. Many default profiles already use a value in this range.
- Print a 20 mm cube and measure across the bottom layers and higher up with calipers. If the bottom is still wider, raise the value by 0.05 mm; if the bottom edge looks pinched inwards, lower it.
- Fix Z offset and bed temperature first. Compensation hides a small, even lip; it can’t hide a first layer that’s being crushed.
Where to find these settings in your slicer
| Setting | OrcaSlicer / Bambu Studio | PrusaSlicer | Cura |
|---|---|---|---|
| Elephant foot compensation | Process → Quality → Precision → Elephant foot compensation (Advanced mode; a positive value shrinks the first layer) | Print Settings → Advanced → Elephant foot compensation (Advanced or Expert mode) | Initial Layer Horizontal Expansion, in Walls (Shell in older versions); use a negative value, e.g. −0.1 mm |
| Bed temperature | Filament settings → Bed temperature (per plate type) | Filament Settings → Filament → Bed | Material → Build Plate Temperature |
| First-layer nozzle temperature | Filament settings → Nozzle temperature → Initial layer | Filament Settings → Filament → Temperature → First layer | Material → Printing Temperature Initial Layer |
| First-layer line width | Process → Quality → Line width → First layer | Print Settings → Advanced → Extrusion width → First layer | Quality → Initial Layer Line Width |
| Flow | Filament settings → Flow ratio | Filament Settings → Filament → Extrusion multiplier | Material → Flow |
| Fan off for first layers | Filament settings → Cooling → No cooling for the first layers | Filament Settings → Cooling → Disable fan for the first layers | Cooling → Initial Fan Speed and Regular Fan Speed at Layer |
Menu names move between slicer versions. If you can’t find a setting, type its name into the slicer’s settings search box.
The first few layers.
Layer 1 of 225, z 0.2 mm.
Layer 10 of 225, z 2.0 mm.
Layer 25 of 225, z 5.0 mm.
Benchy cut open: walls, infill and overhangs in one small boat.Photo: CreativeTools: https://www.thingiverse.com/Cr… ·CC0 ·Wikimedia Commons
Gyroid infill in a slicer preview.Photo: Anachronist ·CC BY-SA 4.0 ·Wikimedia Commons
Step 7: Add a chamfer to the bottom edge
If you design your own parts, a small chamfer (an angled cut) on the bottom edge hides any remaining lip completely. A 0.5–1 mm chamfer at 45° is enough: the bulge fills the cut-away space instead of sticking out past the wall.
This is the most reliable fix for parts that must fit exactly at the base, like lids, boxes that stack, or pegs that go into holes.
A screw-top box: threads print well at 0.2 mm layers.Photo: syvwlch ·CC BY 2.0 ·Wikimedia Commons
A printed maze puzzle.Photo: Sumanbargavr ·CC BY-SA 4.0 ·Wikimedia Commons
A working wrench printed in one piece.Photo: Creative Tools from Halmdstad, Sweden ·CC BY 2.0 ·Wikimedia Commons
A table of small prints.Photo: Trevor Prentice ·CC BY-SA 2.0 ·Wikimedia Commons
Settings by material
| Material | Prone to elephant’s foot? | Bed | Notes |
|---|---|---|---|
| PLA | Medium | 50–65 °C | Glass transition about 60 °C; a cooler bed often fixes it |
| PETG | Medium | 70–85 °C | Sticks hard; raise Z offset a little rather than squishing it |
| ABS / ASA | Medium–high | 90–110 °C | The bed must stay hot to stop warping, so rely on compensation |
| TPU | High | 30–60 °C | Soft and squashy by nature; print slowly and keep the bed cool |
If you’ve changed printers or slicers, start from the manufacturer’s profile for that filament before tuning anything else.
PLA: the beginner's filament.Photo: Richardspa ·CC0 ·Wikimedia Commons
A 1 kg spool of PETG, sealed with desiccant.Photo: Suit ·CC BY-SA 4.0 ·Wikimedia Commons
A spool of ABS.Photo: Tatár Lehel ·CC BY-SA 3.0 ·Wikimedia Commons
Flexible filament: label shows its print temperature.Photo: Sweetclara ·CC BY-SA 4.0 ·Wikimedia Commons
When elephant’s foot won’t go away
If you’ve worked through every step and the lip is still there:
- Reset to the stock profile and change one setting at a time. Several half-tuned first-layer settings can stack up.
- Check the Z offset again after a nozzle change. A new nozzle can sit at a slightly different height, which changes the gap.
- Check the bed surface. A textured sheet hides a small lip better than a smooth one, and swapping sheets can change the gap if they’re different thicknesses.
- Look for a heavy raft or brim. A brim doesn’t cause elephant’s foot, but plastic left behind when you remove it can look like one. Trim it with a deburring tool or a flat file.
- Accept a tiny lip on functional parts and file it. A few passes with a deburring tool or fine sandpaper removes a small bulge in seconds.
A scraper: lift prints off a rigid bed.Photo: syvwlch ·CC BY 2.0 ·Wikimedia Commons
The nozzle threads into the heater block.Photo: syvwlch ·CC BY 2.0 ·Wikimedia Commons
A Z motor turns the lead screw through a coupler.
The Z lead screw lifts the gantry.Photo: kenming Wang ·CC BY-SA 2.0 ·Wikimedia Commons
Your action plan
- Raise the Z offset until the first layer is slightly flattened, not crushed.
- Lower the bed temperature in 5 °C steps to the coolest value that still holds.
- Reset first-layer flow to 100 % and line width to a normal value.
- Let the part-cooling fan come on from layer 2 or 3.
- Re-level the bed if the lip is uneven.
- Turn on elephant foot compensation at 0.1–0.2 mm and fine-tune with a cube.
- Chamfer the bottom edge of parts you design.
FAQ
What causes elephant’s foot in 3D printing?
The bottom layers are squished too much or kept too soft. The usual causes are a nozzle too close to the bed, a bed that’s too hot, too much plastic on the first layer, and the fan staying off for too long. The weight of the layers above then pushes the soft base outwards.
What is a good elephant foot compensation value?
Start at 0.1–0.2 mm, then print a small cube and measure the bottom with calipers. Increase in 0.05 mm steps if the base is still wider than the walls, and reduce it if the bottom edge looks pinched inwards.
Does a hotter bed cause elephant’s foot?
It can. A bed near or above the plastic’s glass transition keeps the bottom layers soft, so they sag under the weight of the print. Use the coolest bed temperature that still holds your part to the end of the print.
Is elephant’s foot the same as over-extrusion?
No. Elephant’s foot only affects the bottom few layers. Over-extrusion puts too much plastic on every layer, so the whole part is oversized and lumpy. If your walls are bumpy all the way up, calibrate flow first.
Can I fix elephant’s foot in Cura?
Yes. Cura doesn’t call it elephant foot compensation; the setting is Initial Layer Horizontal Expansion. Set it to a negative value, such as −0.1 mm, to shrink the outline of the first layer; a positive value makes the foot worse. The easiest way to find it is to type “horizontal expansion” into the settings search box, since the section it sits in has changed between Cura versions.
Why does elephant’s foot only appear on one side of my print?
The bed isn’t level, so the nozzle is closer to the bed on that side. Re-level the bed or re-run auto bed leveling, then check the Z offset again.
Will raising the Z offset make my first layer stop sticking?
It can if you raise it too far. Raise it in 0.02–0.05 mm steps and stop when the lines are still slightly flattened and touch each other. That’s enough squish for adhesion without pushing the outer wall outwards.
Related guides
Elephant’s foot is one of several print-quality problems; for another one, see how to fix stringing. To get the first layer right, read what Z offset is and how to set it, how to level a 3D printer bed and first layer not sticking. If you fix it with a cooler bed and the corners start to lift, see how to fix warping. New to printing? Start with the complete beginner’s guide.